强化玻璃板的制造方法;METHOD FOR MANUFACTURING TEMPERED GLASS PLATE
摘要
本发明的强化玻璃板的制造方法的特征在于包括:排列步骤,将大致矩形且板厚1.0mm以下的强化用玻璃板,以直立姿势且在厚度方向上隔开10mm以下的间隔而在支持体上排列多个,从而获得强化用玻璃板排列体;强化步骤,将强化用玻璃板排列体浸渍于离子交换溶液中,进行离子交换处理,而获得强化玻璃板排列体;缓冷步骤,将强化玻璃板排列体自离子交换溶液中取出后进行缓冷;以及取出步骤,将构成强化玻璃板排列体的各强化玻璃板自支持体中取出。; a tempering step in which the glass plate for temper-arranged body is dipped in an ion exchange solution to perform an ion exchange treatment so as to obtain a tempered glass plate-arranged body; a slow cooling step in which the tempered glass plate-arranged body is taken out from the ion exchange solution for slow cooling; and a taking-out step in which each tempered glass plate which constructs the tempered glass plate arranged-body is taken out from the support.