摘要 |
The present invention relates to a method for the production calcium sulfoaluminate (belite, ferrite, ternesite) clinker using fluxes/mineralizers comprising the following steps - providing a raw meal comprising at least sources of CaO, AI2O3, SO3 - sintering the raw meal in a kiln at 1100 to 1350 °C to provide a clinker, - cooling the clinker, wherein at least one compound containing copper and a glass powder or a glass powder are added prior to sintering. The invention further relates to the clinker obtained, as well as to calcium sulfoaluminate based cements and binders produced from the clinker. |