摘要 |
<p><P>PROBLEM TO BE SOLVED: To provide a composition for water-based coating allowing forming a coating film without white turbidity, without blending special additives. <P>SOLUTION: The composition for water-based coating contains: a fluorine-containing copolymer (A) with an acid value of 10-30 mgKOH/g having a functional group reactive with an isocyanate group; block polyisocyanate (B) blocked by a compound represented by a formula (1); and water. In the formula (1), R is a 1-5C alkyl group or a 1-5C alkoxy group, and R<SP POS="POST">1</SP>is a 1-5C alkyl group. <P>COPYRIGHT: (C)2013,JPO&INPIT</p> |