摘要 |
<p>PROBLEM TO BE SOLVED: To provide a transparent conductive laminate excellent in flatness, in which an electrode pattern can be formed with high accuracy by post-processing on both surfaces of the laminate, and to provide a method for manufacturing the transparent conductive laminate.SOLUTION: The method for manufacturing a transparent conductive laminate 30 comprises: a step of laminating a first transparent conductive film 10 having at least a hard coat layer 2, 2' and a transparent conductive layer 3, 3' successively deposited on at least one surface of a transparent substrate film 1, 1' with a second transparent conductive film 20 having the similar constitution via an adhesive layer 4 in such a manner that faces of the above films where the transparent conductive layer 3, 3' is not deposited oppose to each other; and a step of heat treating the laminate. A difference in the maximum thermal shrinkage of the laminate is within 0.2% in an oblique direction at an angle of 45 degrees from a flow direction that coincides with flow directions of the first transparent conductive film 10 and of the second transparent conductive film 20 when these films are laminated.</p> |