发明名称 |
TONER PROCESS COMPRISING REDUCED COALESCENCE TEMPERATURE |
摘要 |
A method of forming toner particles includes aggregating a mixture of a latex, a wax, and an optional pigment to form pre-toner particles, and coalescing the pre-toner particles at a substantially constant target temperature selected within a range from about the glass transition temperature of the pre-toner particles to about 75° C., thereby creating toner particles having a substantially constant particle size distribution during the coalescing step. |
申请公布号 |
US2015056551(A1) |
申请公布日期 |
2015.02.26 |
申请号 |
US201313972360 |
申请日期 |
2013.08.21 |
申请人 |
XEROX CORPORATION |
发明人 |
Schneider Jay Lee;Sheik-Qasim Abdisamed;Tin Randy Pheav;Wolfe Christopher Michael;Veregin Richard Philip Nelson;Elliott Mark;Davis Melanie;Vong Cuong;Qiu Shigang Steven |
分类号 |
G03G9/08 |
主分类号 |
G03G9/08 |
代理机构 |
|
代理人 |
|
主权项 |
1. A method of forming toner particles comprising:
aggregating a mixture comprising a latex, a wax, and an optional pigment to form pre-toner particles; and coalescing the pre-toner particles at a substantially constant target temperature selected within a range from about the glass transition temperature of the pre-toner particles to about 75° C., thereby creating toner particles having a substantially constant particle size distribution during the coalescing step. |
地址 |
Norwalk CT US |