发明名称 Sintered cubic boron nitride compact and sintered cubic boron nitride compact tool
摘要 It is an object of the present invention to provide a sintered cBN compact having excellent wear resistance and fracture resistance even in machining centrifugally cast iron having a property of being difficult to machine, and to provide a sintered cBN compact tool. A sintered cBN compact of the present invention contains 20% by volume or more and 65% by volume or less of cBN and, as a binder, 34% by volume or more and less than 80% by volume of Al2O3, at least one selected from the group consisting of nitrides, carbides, carbonitrides, borides, and boronitrides of Zr and solid solutions thereof (hereinafter, referred to as “X”), and ZrO2, the total amount of X and ZrO2 being 1.0% by volume or more and 6.0% by volume or less, the volume ratio of ZrO2 to Al2O3, ZrO2/Al2O3, being 0.010 or more and less than 0.100, in which the ratio Itetragonal ZrO2(101)/IαAl2O3(110) is 0.1 or more and 3 or less, where Itetragonal ZrO2(101) is the intensity of the (101) plane of tetragonal ZrO2 and IαAl2O3(110) is the intensity of the (110) plane of αAl2O3 among X-ray diffraction peaks of the sintered cBN compact.
申请公布号 US8962505(B2) 申请公布日期 2015.02.24
申请号 US201113700041 申请日期 2011.10.26
申请人 Sumitomo Electric Hardmetal Corp. 发明人 Okamura Katsumi;Abe Machiko;Kukino Satoru
分类号 C04B35/5831;C04B35/119;C04B35/10;C04B35/117;C04B35/63 主分类号 C04B35/5831
代理机构 Ditthavong & Steiner, P.C. 代理人 Ditthavong & Steiner, P.C.
主权项 1. A sintered cBN compact, containing: 20% by volume or more and 65% by volume or less of cBN relative to the whole sintered compact; as a binder, 34% by volume or more and less than 80% by volume of Al2O3 relative to the whole sintered compact, and ZrC; and ZrO2, wherein the total amount of ZrC and ZrO2 being 1.0% by volume or more and 6.0% by volume or less relative to the whole sintered compact, the volume ratio of ZrO2 to Al2O3, ZrO2/Al2O3, being 0.010 or more and less than 0.100; wherein the ratio Itetragonal ZrO2(101)/IαAl2O3(110) is 0.1 or more and 3 or less, where Itetragonal ZrO2(101) is the intensity of the (101) plane of tetragonal ZrO2 and IαAl2O3(110) is the intensity of the (110) plane of αAl2O3 among X-ray diffraction peaks of the sintered cBN compact; and wherein the content of the ZrC in the sintered cBN compact is 0.1% by volume or more and 3.0% by volume or less.
地址 Hyogo JP