发明名称 正極活物質
摘要 <p><P>PROBLEM TO BE SOLVED: To provide a method for manufacturing iron lithium phosphate with fine and uniform grain sizes and excellent discharge and charge characteristics of a secondary battery to be obtained in high purity and in high yield. <P>SOLUTION: The method for manufacturing iron lithium phosphate is characterized in that a reducing compound is added after mixing a lithium compound, a phosphoric acid compound and water so that an oxidation/reduction potential of the mixture in a reducing atmosphere is less than -1 mV, and then, a divalent iron compound is added and the mixture is subjected to hydrothermal reaction. <P>COPYRIGHT: (C)2013,JPO&INPIT</p>
申请公布号 JP5673953(B2) 申请公布日期 2015.02.18
申请号 JP20110192457 申请日期 2011.09.05
申请人 发明人
分类号 C01B25/45;H01M4/58 主分类号 C01B25/45