发明名称 |
METHOD AND THERMOPLASTIC FOAMED ARTICLE |
摘要 |
A method for making a low density foamed article includes placing a desired amount of thermoplastic polyurethane foam beads in a cavity of an injection mold and closing the mold; combining in an extruder connected to the mold a molten polymer selected from the group consisting of thermoplastic polyurethane elastomers and thermoplastic ethylene-vinyl acetate copolymers with both a physical or chemical blowing agent other than a supercritical fluid present in an amount up to about 15 wt % based on molten polymer weight and a supercritical fluid that is at least one of about 0.1 to about 5 weight percent of supercritical CO2 based on molten polymer weight or about 0.1 to about 4 weight percent of supercritical N2 based on molten polymer weight, to form a mixture and injecting the mixture into the mold and foaming the mixture to form the low density foamed article. |
申请公布号 |
US2015038607(A1) |
申请公布日期 |
2015.02.05 |
申请号 |
US201313958531 |
申请日期 |
2013.08.02 |
申请人 |
NIKE, Inc. |
发明人 |
Baghdadi Hossein A. |
分类号 |
B29C44/02;C08J9/228 |
主分类号 |
B29C44/02 |
代理机构 |
|
代理人 |
|
主权项 |
1. A method for making a low density foamed article, comprising:
placing a desired amount of thermoplastic polyurethane foam beads in a cavity of a mold and closing the mold; combining in an extruder connected to the mold a molten polymer selected from the group consisting of thermoplastic polyurethane elastomers and thermoplastic ethylene-vinyl acetate copolymers with (a) a physical or chemical blowing agent other than a supercritical fluid and (b) a supercritical fluid,wherein the blowing agent (a) is present in an amount up to about 15 wt % based on polymer weight and the supercritical fluid comprises at least one of about 0.1 to about 5 weight percent of supercritical CO2 based on polymer weight or about 0.1 to about 4 weight percent of supercritical N2 based on polymer weight, to form a mixture and
injecting the mixture into the mold and foaming the mixture. |
地址 |
Beaverton OR US |