发明名称 Method of manufacturing organic light emitting diode arrays and system for eliminating defects in organic light emitting diode arrays
摘要 A method for manufacturing an organic light emitting diode (OLED) array is provided that includes applying an energizing signal to at least one of the OLED pixels in the array. The energizing signal exceeds a threshold level. The method also includes reducing the energizing signal and identifying an OLED in the array that continues to remain energized. The method further includes irradiating the identified OLED to degrade the organic material in the OLED. A method of performing quality control in a manufacturing process of an OLED array is provided. The method includes determining an intensity, a time and a wavelength of radiation sufficient to render an OLED of the OLED array inoperative by degrading organic material in the OLED. A system of performing quality control in a manufacturing process of an OLED array is provided. A computer-readable medium having stored thereon computer-executable instructions is provided.
申请公布号 US8944873(B2) 申请公布日期 2015.02.03
申请号 US201213484677 申请日期 2012.05.31
申请人 eMagin Corporation 发明人 Ghosh Amalkumar P.
分类号 H01J9/50;H01L51/00;H01L51/56 主分类号 H01J9/50
代理机构 Epstein Drangel LLP 代理人 Epstein Drangel LLP ;Epstein Robert L.
主权项 1. A method of performing quality control in a manufacturing process of an organic light emitting diode (OLED) array comprising OLED pixels, comprising: determining an intensity, a time and a wavelength of radiation sufficient to render an OLED pixel of the OLED array inoperative by degrading organic material in the OLED pixel, the determining operation being based on at least one of a first degradability of the organic material, a first absorption spectrum of the organic material, a second degradability of at least one surface layer of the OLED array, and a second absorption spectrum of the at least one surface layer of the OLED array; identifying a stuck-on OLED pixel of the OLED array; and rendering the stuck-on OLED inoperative by degrading the organic material in the active portion of the stuck-on OLED pixel through irradiation of the stuck-on OLED,wherein the irradiation includes directing one of ultraviolet and visible light at the stuck-on OLED pixel and wherein the one of ultraviolet and visible light is visible light having a wavelength of about one of the following: 365 nm, 405 nm, 488 nm and 555 nm.
地址 Hopewell Junction NY US