摘要 |
<p>The invention provides a laminating body manufacturing method and a laminating body. The laminating body is formed by bonding a laminating film utilizing light-cured resin on a to-be-bonded body with steps. Bubbles and white turbidity can be prevented by bonding the laminating film on the to-be-bonded body provided with steps on the surface. The manufacturing method of the laminating body includes a working procedure of preparing the light-cured resin, wherein the light-cured resin has an energy storage volume that is greater than 1*104Pa and less than 9*104Pa below 24 DEG C and 1Hz and contains, by weight 5 to 10 parts (B) at least one among acrylate monomer with hydroxyl (methyl), 1.5 to 1 part of (C) optic polymerization initiator and 0.2 to 0.8 part of (D) bifunctional cross-linking agent relative to 100 parts of (A) host polymer composed of acrylic acid resin whose acid value is 0 to 33.</p> |