摘要 <p><P>PROBLEM TO BE SOLVED: To provide a glass-reinforced resin composition excellent in thermal stability and mechanical strength, and small in anisotropy of mold shrinkage factor thereby suppressing warpage. <P>SOLUTION: This glass-reinforced resin composition includes (B) 1-150 pts.wt. of glass flake (component B) with an averaged thickness of 0.2-0.7μm, and (C) 0.0001-1.0 pt.wt. of a surface-treatment deactivator (component C), based on (A) 100 pts.wt. of a thermoplastic resin (component A), wherein the amount of a surface-treating agent of the glass flake is 1.5-5 pts.wt. based on 100 pts.wt. of the glass flake. <P>COPYRIGHT: (C)2013,JPO&INPIT</p>