发明名称 Disposal method for entirely recycling solid refuse
摘要 A disposal method for entirely recycling solid refuse includes the following steps: sorting, crushing, drying, pressing with high pressure to shaped articles, producing charcoal from combustible refuse in high temperature and firing incombustible refuse in high temperature, at last cooling high temperature articles to obtain solid fuel with various shapes and bricks or board used for building. The method achieves entirely recycling house refuse, especial solid refuse. The method recycles solid refuse to obtain fuel and building material with economic value. The method is simple and its processing cost is low.
申请公布号 US8936738(B2) 申请公布日期 2015.01.20
申请号 US200812670403 申请日期 2008.07.21
申请人 发明人 Lian Qihui
分类号 B09B3/00;C04B33/132;C04B33/135;C04B35/626;C10B53/00;C10B53/08;C10L5/36;C10L5/46;C10L9/08;B03B9/06;C04B18/04 主分类号 B09B3/00
代理机构 Global IP Services 代理人 Gu Tianhua;Global IP Services
主权项 1. A method for entirely recycling solid refuse comprising combustible and incombustible components, the method comprising: sorting the solid refuse into combustible and incombustible refuse categories; dehydrating each of the combustible and incombustible refuse categories using water extractors; crushing each of the dehydrated combustible and incombustible refuse categories into smaller pieces using disintegrators; drying each of the crushed combustible and incombustible refuse categories; pressing and shaping each of the dried combustible and incombustible refuse categories into articles having various shapes using presses applying high pressure, the press for combustible refuse also applying a high temperature selected to prevent combustible refuse from sticking thereto; carbonizing the pressed and shaped combustible refuse at a temperature between 300° C. and 1300° C. for a time between 5 seconds and 18 minutes so as to form charcoal and briquette having various shapes; firing the pressed and shaped incombustible refuse at a temperature between 700° C. and 1200° C. for a time between 1 hour and 10 hours so as to form building bricks or boards having various shapes; and cooling the charcoal, briquette, and bricks or boards so as to obtain finished products.
地址