摘要 |
A process for preparing a thermoplastic polymer composition or a thermoplastic polymer blend, comprising: - from 20 to 80 % by weight of at least one water-moist elastomer component A containing up to 40 %, preferably up to 30 % by weight of residual water, - from 20 to 80 % by weight of at least one thermoplastic polymer B, - from 0 to 40 % by weight of at least one further polymer C, and - from 0 to 60% by weight of additive(s) D, by mixing the elastomer component A with the thermoplastic polymer B and, if present, the further polymer C and, if present, the additive(s) D in an extruder, comprising the steps of precipitating the elastomer component A, and mechanical dewatering of the elastomer component A leads to improved salt-free products. |
申请人 |
STYROLUTION GROUP GMBH |
发明人 |
NIESSNER, NORBERT;BANASZAK, BRIAN J.;VERSTRAETEN, RUDY;MICHELS, GISBERT;FISCHER, WOLFGANG;RUTHARD, CHRISTIAN;JANSEN, ULRICH |