发明名称 微細で低嵩密度の金属ニッケル粉末を生成する方法
摘要 <p>A method of producing a fine, low bulk density nickel powder, comprising a) charging particles of at least one reducible nickel salt within a furnace so as to form a moving bed of furnace charge, and b) reducing the furnace charge with a H<SUB>2</SUB> containing gas at a temperature ranging from about 300°C to about 500°C, the bed of furnace charge being moved gently so as to minimise formation of hard agglomerates and obtaining a fine, low bulk density nickel powder. A similar method, wherein the furnace charge is static and contained within a shallow bed.</p>
申请公布号 JP5650632(B2) 申请公布日期 2015.01.07
申请号 JP20110269857 申请日期 2011.12.09
申请人 发明人
分类号 B22F9/22 主分类号 B22F9/22
代理机构 代理人
主权项
地址