摘要 |
PROBLEM TO BE SOLVED: To provide conductive paper having excellent shield properties of 30 to 60 dB in a frequency range of 1 to 1000 MHz due to its metalization rate of almost 100% as well as excellent heat resistance and processability and provide a manufacturing method thereof in a low cost.SOLUTION: The conductive paper can be formed by mixing a wood pulp coated with electroless metal plating and a wood pulp without metal coating, and papering the mixed pulps. A weight ratio of the metal-coated wood pulp to the total weight of both of the wood pulps is from 53 to 93%. |