发明名称 処理溶液の生成方法、酸性電気めっき浴の生成方法、および、電気めっき皮膜形成方法
摘要 PROBLEM TO BE SOLVED: To provide a technology capable of forming a composite plating coating having uniform particle diameter at nanometer size and containing 10 wt.% or more of molybdenum disulfide.SOLUTION: A molybdenum disulfide derivative solution is produced by addition reaction of tetra thio ammonium molybdate and sodium 2-propyne-1-sulfonate. Then an electroplating coating is formed by using an acidic electroplating bath containing the solution. Since metals such as nickel, copper, and cobalt in the plating bath do not deposit even when the molybdate derivative solution is added to the acidic electroplating bath, a composite plating coating of molybdenum disulfide and metals in the plating bath can be formed by the acidic electroplating bath containing the solution. This enables forming a composite plating coating containing molybdenum disulfide of 10 wt.% or more with having uniform particle diameter at nanometer size.
申请公布号 JP5934872(B2) 申请公布日期 2016.06.15
申请号 JP20130221794 申请日期 2013.10.25
申请人 ユケン工業株式会社 发明人 石崎 伸治;伊藤 和生
分类号 C25D15/02;C25D5/18 主分类号 C25D15/02
代理机构 代理人
主权项
地址