发明名称 改質アスファルト組成物、アスファルト混合物およびアスファルト舗装材
摘要 PROBLEM TO BE SOLVED: To provide a modified asphalt composition, an asphalt mixture and an asphalt pavement material, which are excellent in work efficiency during production or pavement execution, excellent in rut resistance, crack resistance, water resistance or the like as asphalt pavement, and further excellent in long-term storage stability and uniformity. SOLUTION: This modified asphalt composition contains 100 pts. wt asphalt (A), and 1-20 pts. wt modified polyethylene (B) formed by grafting an unsaturated silane compound to polyethylene as much as 0.1-5 wt%, wherein, in the modified polyethylene (B), a melt flow rate measured by 21.16N load at 190°C based on JIS-K7210 (1999) is 2-100 g/10 min., and a melting peak temperature by a differential scanning calorimeter is 100-140°C. COPYRIGHT: (C)2012,JPO&INPIT
申请公布号 JP5644422(B2) 申请公布日期 2014.12.24
申请号 JP20100262976 申请日期 2010.11.25
申请人 发明人
分类号 C08L95/00;C08L51/06;E01C7/22 主分类号 C08L95/00