发明名称 Golf ball with resin inner core having specified coefficient of restitution of the inner core at various speeds
摘要 A high performance golf ball includes a resin inner core, a rubber outer core, and a cover. The resin inner core is made of a blend of highly neutralized polymers and a low flexural modulus ionomer, and may include a blend of different highly neutralized polymers. The inner core has a specified range of coefficients of restitution when measured at different velocities. The cover is a single layer ionomer cover, and may be made from a blend of different grades of the ionomer. The ball as a whole has properties to maximize performance and aesthetic properties, such as backspin off the irons, feel, and sound.
申请公布号 US8911306(B2) 申请公布日期 2014.12.16
申请号 US201213584068 申请日期 2012.08.13
申请人 NIKE, Inc. 发明人 Ichikawa Yasushi;Molinari Arthur;Chou Chien-Hsin;Liu Chen-Tai;Ichinose Jun
分类号 A63B37/04;A63B37/00 主分类号 A63B37/04
代理机构 Honigman Miller Schwartz and Cohn, LLP 代理人 Honigman Miller Schwartz and Cohn, LLP ;Budde Anna M.;O'Brien Jonathan P.
主权项 1. A golf ball comprising: an inner core layer, wherein the inner core layer comprises a first highly neutralized polymer with a first flexural modulus, a second highly neutralized polymer with a second flexural modulus, and a low flexural modulus ionomer, and wherein the inner core layer has a diameter between about 24 mm and about 30 mm; an outer core layer, wherein the outer core layer surrounds and encompasses the inner core layer, and wherein the outer core layer comprises a rubber composition; and a cover layer, wherein the cover layer surrounds and encompasses the outer core layer, wherein the first highly neutralized polymer is about 20 to 60 parts by weight of the inner core layer, wherein a ratio of the second flexural modulus to the first flexural modulus is less than 2, wherein the low flexural modulus ionomer has a flexural modulus of less than about 8,000 psi, wherein the low flexural modulus ionomer is from about 1 to about 50 parts by weight of the inner core layer, wherein the inner core layer has a first coefficient of restitution measured at 131 ft/s of about 0.810 to about 0.835, a second coefficient of restitution measured at 140 ft/s of about 0.805 to about 0.815, and a third coefficient of restitution measured at 160 ft/s of about 0.775 to about 0.790, where an average of the first coefficient of restitution, the second coefficient of restitution, and the third coefficient of restitution is at least 0.8.
地址 Beaverton OR US