发明名称 Molding compositions comprising polyaryl ether with improved surface quality
摘要 A thermoplastic molding composition, comprising: A) from 40 to 97.9% by weight of at least one polyether sulfone,B) from 2 to 59.9% by weight of at least one polysulfone,C) from 0.1 to 2% by weight of stearic acid, and also, if appropriate, further additives and auxiliaries, has improved flowability, surface quality, and notched impact resistance, and can be used for the construction of headlamps.
申请公布号 US8906992(B2) 申请公布日期 2014.12.09
申请号 US200812666106 申请日期 2008.06.19
申请人 BASF SE 发明人 Weber Martin;Bluhm Rüdiger;Maletzko Christian;Lange Gerhard;Erbes Jörg
分类号 C08K5/09;C08K5/098;C08K5/101;C08G75/23;C08L81/06 主分类号 C08K5/09
代理机构 Drinker Biddle & Reath LLP 代理人 Drinker Biddle & Reath LLP
主权项 1. A thermoplastic molding composition, comprising: A) from 45 to 84.8% by weight of at least one polyether sulfone whose glass transition temperature is greater than 200° C. and comprising repeat units of the formula (I):in which t and q, independently of one another, are 0, 1, 2, or 3, each of Q, T, and Z, independently of the others, is a chemical bond or a group, selected from —O—, —S—, —SO2—, S═O, C═O, N═N—, with the proviso that at least one of the groups T, Q and Z is —SO2— and, if t and q are 0, Z is —SO2—, each of Ar and Ar1, independently of the other, is a C6-C18-arylene group, where this can have substitution by C1-C12-alkyl groups, by C6-C18-aryl groups, by C1-C12-alkoxy groups or by halogen atoms, B) from 15 to 54.8% by weight of at least one polysulfone having a glass transition temperature from 170° C. to 195° C. and comprising repeat units of the formula (II):in which R1 is H or C1-C4-alkyl, each of Ar2 and Ar3, independently of the other, is a C6-C12-arylene group, and Y is —SO2—, C) from 0.1 to 1.75% by weight of stearic acid, salts of stearic acid, esters of stearic acid, and/or stearates.
地址 Ludwigshafen DE
您可能感兴趣的专利