Disclosed is a pouch having at least one sealed compartment containing a first composition. At least one wall of the at least one sealed compartment is made from a water-soluble film having any suitable thickness. The water-soluble film comprises PVOH polymer such that when the film has a thickness of about 76 microns the film is characterized by a Dissolution Index of about 620 to about 920, or of about 665 to about 920, or about 710 to about 920; and a Stress Index of about 145 to about 626, or about 155 to about 480, or about 165 to about 325. |
申请公布号 |
US8905236(B2) |
申请公布日期 |
2014.12.09 |
申请号 |
US201113016621 |
申请日期 |
2011.01.28 |
申请人 |
Monosol, LLC |
发明人 |
Denome Frank W.;Friedrich Steven G.;Labeque Regine;Lee David M.;Rosmaninho Roxane;Shi Jichun;Verrall Andrew P. |
分类号 |
B65D85/84;C08J5/18;C11D17/04;C08L29/04;B65D65/46 |
主分类号 |
B65D85/84 |
代理机构 |
Marshall, Gerstein & Borun LLP |
代理人 |
Marshall, Gerstein & Borun LLP |
主权项 |
1. A water-soluble film having any suitable thickness, the water-soluble film comprising:
at least 50 wt. % of a water-soluble polyvinyl alcohol (PVOH) resin, the PVOH resin having an average viscosity in a range of about 13.5 cP to about 20 cP and a degree of hydrolysis in a range of about 84% to about 92%; and the film further having no more than 30 wt. % of a PVOH polymer having an average viscosity less than about 11 cP; the film further characterized by having a Dissolution Index in a range of about 620 to about 920 and a Stress Index in a range of about 145 to about 626 when the film has a thickness of about 76 microns, wherein the film is thermoformable. |