发明名称 STEEL HAVING ACID DEW CORROSION RESISTANCE, AND EXHAUST GAS FLOW PATH CONSTITUENT MEMBER
摘要 <p>A steel has improved sulfuric acid dew point corrosion resistance without relying upon the addition of Sb and can have improved hydrochloric acid dew point corrosion resistance. The acid dew point corrosion-resistant steel includes from 0.005 to 0.200% of C, from 0.20 to 0.80% of Si, from 0.05 to 1.50% of Mn, from 0.002 to 0.020% of P, from 0.005 to 0.015% of S, from 0.10 to 0.50% of Cu, from 0.05 to 0.30% of Ni, from 0.005 to 0.100% of Al, and 0 or more and less than 0.010% of Mo in terms of % by mass, with the balance being Fe and impurities. In the case of attaching great importance to hydrochloric acid dew point corrosion resistance, it is desirable to control the Mo content in the foregoing steel to from 0.005 to 0.030% by mass.</p>
申请公布号 KR20140138770(A) 申请公布日期 2014.12.04
申请号 KR20147026731 申请日期 2012.03.19
申请人 NISSHIN STEEL CO., LTD. 发明人 KATAGIRI YUKIO;MORIKAWA SHIGERU;FUJIWARA SUSUMU
分类号 C22C38/08;C22C38/16;F23J13/02 主分类号 C22C38/08
代理机构 代理人
主权项
地址