To a solid backer (1) is attached foil (3), be filled with an insulating material (5) and carried out surface treatment, for example facade. By fulfilling of one container (6) are supplying cellulose particles and from second container (7)liquid mixture based on water and polymer. It is formed a slurry hardening at 5 to 40 � C, the surface of which aligns in still plastic condition. Assembly of the parts of the cellular foil (3) of different heights and / or a laminating, and / or is formed by bending the surface of cladding. The insulating layer has a structure of flexible plastic chambers filled with insulating material (5) bonded to the backer (1) and the cell walls, preferably based on cellulosic particles and the aqueous dispersion of styrene acrylate copolymer, with a size of up to 1 cm, and an amount of 70 to 90 vol.%, wherein the insulation material (5) extend to the edge of the cells, or through, and is covered with a surface layer (10). Parts of the cellular foil (3) with various high lined up form or pushing on the building projections. |