<p>The present invention relates to a method for manufacturing a brick for a building interior material, comprising: a step of preparing a composition by mixing a fiber-reinforced plastic hardener and a stone dust mixed liquid at the weight ratio of 1:1-5:1; a step of preparing a mixture by adding 5-20 parts by weight of flame retardant Styrofoam pellets as an additive to 80-95 parts by weight of the prepared composition; a step of stirring the prepared mixture at room temperature to 50 degrees Celsius for 1-2 hours; and a step of hardening the stirred mixture by filling a brick mold with the stirred mixture.</p> |