摘要 |
The present invention relates to a mixture for producing a layer in a layer structure, comprising: a) 0.1-10 parts by weight of metal particles of a median particle size D50 of 2-20 µm; b) 1-70 parts by weight of a first solvent having a boiling point of above 100°C and a vapour pressure of 1-15 hPa (20°C); and c) 30-70 parts by weight of a second solvent having a boiling point of below 100°C and a vapour pressure of 20-200 hPa (20°C), and also use thereof in a method for producing a layer structure, the said layer structure, and use thereof, in particular for coating boat hulls. |