发明名称 |
LIGHTWEIGHT INFILLING MORTAR COMPOSITION |
摘要 |
PROBLEM TO BE SOLVED: To provide a lightweight infilling mortar composition having excellent fillability, capable of being integrated with an existing member made of steel by being filled into the inside space of a hollow member such as a steel plate deck U rib as reinforcement for a steel plate deck and eliminating unfilled parts caused by air reservoirs as possible, and a lightweight infilling mortar.SOLUTION: Provided is a lightweight infilling mortar composition comprising cement and a lightweight aggregate. The lightweight infilling mortar composition is characterized in that flow value (no fall motion) after the removal of flow cones using flow cones prescribed in a flow test in JIS R 5201 {a physical test method for cement} 11 is 125 to 185 mm, and also, flow-down time in {a fluidization test method (plan) for infilling mortar} in the Civil Engineering Standards JSCE-F541-2010 cannot be measured by the clogging of the mortar. Also provided is a lightweight infilling mortar using the same. |
申请公布号 |
JP2014221702(A) |
申请公布日期 |
2014.11.27 |
申请号 |
JP20130102194 |
申请日期 |
2013.05.14 |
申请人 |
HANSHIN EXPRESSWAY CO LTD;HANSHIN EXPRESSWAY TECHNOLOGY CENTER;TAIHEIYO MATERIAL KK |
发明人 |
SUGIYAMA HIROKI;TANBA NORIO;SHIBAGAKI MASANORI;NAKAHARA KAZUHIKO |
分类号 |
C04B28/02;C04B14/18;C04B22/04;C04B22/06;C04B24/38 |
主分类号 |
C04B28/02 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|