发明名称 METHOD FOR PRODUCING AUSTENITIC STAINLESS STEEL AND AUSTENITIC STAINLESS STEEL MATERIAL
摘要 Austenitic stainless steel having high temperature strength and excellent nitric acid corrosion resistance is provided. The austenitic stainless steel according to the present embodiment including, in mass percent, C: at most 0.050%, Si: 0.01 to 1.00%, Mn: 1.75 to 2.50%, P: at most 0.050%, S: at most 0.0100%, Ni: 20.00 to 24.00%, Cr: 23.00 to 27.00%, Mo: 1.80 to 3.20%, and N: 0.110 to 0.180%, the balance being Fe and impurities, a grain size number of crystal grains based on JIS G0551 (2005) is at least 6.0, and an area fraction of a à phase is at most 0.1%.
申请公布号 EP2725113(A4) 申请公布日期 2014.11.26
申请号 EP20120802967 申请日期 2012.06.20
申请人 NIPPON STEEL & SUMITOMO METAL CORPORATION 发明人 UEYAMA, MASAKI
分类号 C22C38/00;C21D6/00;C22C30/00;C22C38/58 主分类号 C22C38/00