摘要 |
<p>The present invention provides a lightweight synthetic resin pipe composition having high strength and a method for producing the same. In the present invention, as raw ingredients, 3-6 parts by weight of an ethylene denatured copolymer, 2-4 parts by weight of a shock alleviating agent, 3-8 parts by weight of a glass plasticized ceramic powder, 5-10 parts by weight of a titan-containing ceramic powder, 1-3 parts by weight of a processing material, and 1-5 parts by weight of a filler are included based on 100 parts by weight of polyvinyl chloride. The glass plasticized ceramic powder is produced by plasticizing a waste glass product at high temperature in order to be made into ceramic, wherein shock resistance and lightweight properties are applied to the synthetic resin pipe composition. Moreover, the titan-containing ceramic powder is produced by mixing magnetite, which is a main ingredient and includes titan components, with minerals including feldspar in order to be plasticized three times or more from low temperature to high temperature.</p> |