发明名称 TREATED INORGANIC PIGMENTS HAVING IMPROVED DISPERSABILITY AND USE THEREOF IN COATING COMPOSITIONS
摘要 The disclosure provides a coating composition comprising a treated inorganic core particle, having improved dispersability, prepared by a process comprising: heating a slurry comprising porous silica treated inorganic core particle and water at a temperature of at least about 90° C., more typically about 93 to about 97° C., still more typically about 95 to about 97° C.; and adding a soluble alumina source to the slurry while maintaining the pH at about 8.0 to 9.5 to form an alumina treatment on the porous silica treated inorganic core particle; wherein the treated inorganic core particle does not comprise dense silica or alumina treatments, and has silica present in the amount of about 7% to about 14% and alumina present in the amount of about 4.0% to about 8.0%; and wherein the particle to particle surface treatments are substantially homogeneous.
申请公布号 US2014343212(A1) 申请公布日期 2014.11.20
申请号 US201214354378 申请日期 2012.10.11
申请人 E I DU PONT DE NEMOURS AND COMPANY 发明人 Diebold Michael Patrick;Kraiter Daniel C.;Rusnak Eric;Shih Agingu
分类号 B01J13/02;C09D7/12;C08K3/00;B01J13/22;C09C1/36 主分类号 B01J13/02
代理机构 代理人
主权项 1. A coating composition comprising a treated inorganic core particle, having improved dispersability, prepared by a process comprising: (a) heating a slurry comprising porous silica treated inorganic core particle and water at a temperature of at least about 90° C.; and (b) adding a soluble alumina source to the slurry from step (a) while maintaining the pH at about 8.0 to 9.5 to form an alumina treatment on the porous silica treated inorganic core particle; wherein the treated inorganic core particle does not comprise dense silica or alumina treatments, and has silica present in the amount of about 7% to about 14% and alumina present in the amount of about 4.0% to about 8.0%; and wherein the particle to particle surface treatments are substantially homogeneous.
地址 Wilmington DE US