发明名称 |
Diamond tools |
摘要 |
A method comprising: selecting a diamond material; irradiating the diamond material to increase toughness and/or wear resistance of the diamond material; and processing the diamond material into one or more diamond tool pieces, wherein the diamond material is selected from the group consisting of: a HPHT diamond material having a total equivalent isolated nitrogen concentration in the range 1 to 600 ppm; a CVD diamond material having a total equivalent isolated nitrogen concentration in the range 0.005 to 100 ppm; and a natural diamond material having a total nitrogen concentration in the range 1 to 2000 ppm, wherein the irradiating comprises controlling energy and dosage of irradiation to provide the diamond material with a plurality of isolated vacancy point defects, the isolated vacancy point defects having a concentration in a range 1×1014 to 1×1021 vacancies/cm−1. |
申请公布号 |
US8890091(B2) |
申请公布日期 |
2014.11.18 |
申请号 |
US201113698644 |
申请日期 |
2011.06.01 |
申请人 |
Element Six Limited |
发明人 |
Twitchen Daniel James;Geoghegan Sarah Louise;Perkins Neil |
分类号 |
C01B31/06;C09K3/14;B24D99/00;C30B33/04;C30B29/04;B24D18/00 |
主分类号 |
C01B31/06 |
代理机构 |
Bryan Cave LLP |
代理人 |
Bryan Cave LLP |
主权项 |
1. A method comprising:
selecting a diamond material; irradiating the diamond material to increase toughness and/or wear resistance of the diamond material; and processing the diamond material into one or more diamond tool pieces, wherein the diamond material is selected from the group consisting of: a HPHT diamond material having a total equivalent isolated nitrogen concentration in the range 1 to 600 ppm; a CVD diamond material having a total equivalent isolated nitrogen concentration in the range 0.005 to 100 ppm; and a natural diamond material having a total nitrogen concentration in the range 1 to 2000 ppm, and wherein the irradiating comprises controlling energy and dosage of irradiation to provide the diamond material with a plurality of isolated vacancy point defects, the isolated vacancy point defects having a concentration in a range 1×1014 to 1×1021 vacancies/cm3. |