发明名称 SILANE CROSSLINKING FIRE-RETARDANT COMPOSITION, AND INSULATED WIRE USING THE SAME
摘要 PROBLEM TO BE SOLVED: To provide a fire-retardant composition excellent in heat resistance, fire retardancy and thermal deformability.SOLUTION: A silane crosslinking fire-retardant composition is formed by mixing 20-50 pts.mass of a bromine-based flame retardant, 1-40 pts.mass of antimony trioxide, 1-15 pts.mass of a benzimidazole-based compound, 1-15 pts.mass of zinc oxide, and 0.005-0.3 pts.mass of a silane crosslinking catalyst, based on 100 pts.mass of a resin component. The resin composition contains 5-40 mass% of one or more polypropylene-containing resins selected from a group consisting of 40-80 mass% of a silane modified ethylene-based copolymer resin, a polypropylene-based resin and a polypropylene-based thermoplastic elastomer, with the balance including a polyethylene-based resin.
申请公布号 JP2014214239(A) 申请公布日期 2014.11.17
申请号 JP20130093269 申请日期 2013.04.26
申请人 AUTO NETWORK GIJUTSU KENKYUSHO:KK;SUMITOMO WIRING SYST LTD;SUMITOMO ELECTRIC IND LTD 发明人 SHIRAKI KOSUKE
分类号 C08L23/26;C08K3/22;C08K5/3447;C08L23/04;C08L23/10;H01B3/44;H01B7/02;H01B7/295 主分类号 C08L23/26
代理机构 代理人
主权项
地址