发明名称 REACTOR AND COMPOUND USED IN SAME
摘要 [Problem] Provided is an injection-molded reactor which has excellent heat dissipation properties and in which the internal temperature of the core can be satisfactorily inhibited from rising due to heat generation when the reactor is in operation.;[Solution Means] A material for a core obtained by mixing a soft magnetic powder, a resin binder, and a thermally conductive fibrous filler having a higher thermal conductivity than the soft magnetic powder in accordance with X·(soft magnetic powder)+Y·(thermally conductive filler)+(100-X-Y)·(resin binder), wherein X, indicating the proportion of the soft magnetic powder, is 83 to 96% by mass and Y, indicating the proportion of the thermally conductive filler, is 0.2 to 6.8% by mass, is used to mold a core 16 so that a coil 10 obtained by winding an electric wire is embedded therein without an interval, thereby configuring a reactor 15.
申请公布号 US2014333401(A1) 申请公布日期 2014.11.13
申请号 US201214351534 申请日期 2012.09.19
申请人 Daido Steel Co. Ltd. 发明人 Esaki Junichi;Tozawa Yusuke;Kajinami Yoshitomo;Yoshimoto Kousuke
分类号 H01F27/22;H01F27/32;H01F1/01;H01F27/255 主分类号 H01F27/22
代理机构 代理人
主权项 1. A reactor, wherein a material for a core obtained by mixing a soft magnetic powder, a resin binder and a thermally conductive fibrous filler having a higher thermal conductivity than that of the soft magnetic powder, in a proportion represented by the following expression (1); and the core is molded by using the material for a core in a state where a coil in which a conductor wire is wound is embedded in an inner portion without an interval to configure the reactor, X·(soft magnetic powder)+Y·(thermally conductive filler)+(100-X-Y)·(resin binder)  expression (1) wherein X is 83 to 96% by mass and Y is 0.2 to 6.8% by mass.
地址 Nagoya-shi, AICHI JP