摘要 |
<p>The present disclosure provides a plastic glazing comprising: a base layer; and a coating layer formed on one surface of the base layer, wherein the base layer comprises polycarbonate containing a biphenyl group and the biphenyl group is present in an amount of 10 mol% to 50 mol% based on the total amount of polycarbonate.</p> |