Polymer compositions for blow molding applications
摘要
A polymer having a density of from about 0.950 g/cc to about 0.955 g/cc and a melt index of from about 0.2 g/10 min. to about 0.6 g/10 min., wherein an article formed from the polymer has an environmental stress crack resistance of equal to or greater than about 2000 hours when measured in accordance with ASTM D 1693 condition B, 100% Igepal.
申请公布号
EP2784097(A3)
申请公布日期
2014.10.29
申请号
EP20140162872
申请日期
2012.06.08
申请人
CHEVRON PHILLIPS CHEMICAL COMPANY LP
发明人
YANG, QING;MCDANIEL, MAX P;BEAULIEU, WILLIAM B;YU, YOULU;CRAIN, TONY R