发明名称 |
METHOD FOR MANUFACTURING DYED WOVEN OR KNITTED FABRIC USING METALLIC YARN AND POLYESTER YARN AND FABRIC MANUFACTURED USING THE METHOD |
摘要 |
A method for manufacturing dyed woven or knitted fabric includes preparing woven or knitted fabric using metallic yarn and normal-pressure dyeing polyester yarn having an elasticity modulus of 400 to 600 kg/mm2 and an elongation of 30 to 40%, fabricating a dye bath by putting a dye solution obtained by dispersing a dye in water, dyeing the woven or knitted fabric by putting the prepared woven or knitted fabric into the fabricated dye bath, raising a temperature of the dye bath starting from 35 to 45° C. for 30 to 50 minutes at a rate of 1.2 to 1.5° C./min, and maintaining the heated dye bath at 90 to 100° C. for 15 to 25 minutes, and washing the dyed woven or knitted fabric. The dyed woven or knitted fabric has a light reflection reduction rate of 20% to 30%. |
申请公布号 |
US2014310889(A1) |
申请公布日期 |
2014.10.23 |
申请号 |
US201214358034 |
申请日期 |
2012.05.30 |
申请人 |
Woo Jung Ha;Kim Sun Jin;Cho Sung Hyun |
发明人 |
Woo Jung Ha;Kim Sun Jin;Cho Sung Hyun |
分类号 |
D06P1/00 |
主分类号 |
D06P1/00 |
代理机构 |
|
代理人 |
|
主权项 |
1. A method for manufacturing dyed woven or knitted fabric, comprising:
preparing woven or knitted fabric using metallic yarn and normal-pressure dyeing polyester yarn having an elasticity modulus of 400 to 600 kg/mm2 and an elongation of 30 to 40%; fabricating a dye bath by putting a dye solution obtained by dispersing a dye in water; dyeing the woven or knitted fabric by putting the prepared woven or knitted fabric into the fabricated dye bath, raising a temperature of the dye bath starting from 35 to 45° C. for 30 to 50 minutes at rate of 1.2 to 1.5° C./min, and maintaining the heated dye bath at 90 to 100° C. for 15 to 25 minutes; and washing the dyed woven or knitted fabric. |
地址 |
Gyeonggi-do KR |