发明名称 Inorganic solid electrolyte glass phase composite and a battery containing an inorganic solid electrolyte glass phase composite
摘要 An inorganic solid electrolyte glass phase composite is provided comprising a substance of the general formula La2/3-xLi3xTiO3 wherein x ranges from about 0.04 to about 0.17, and a glass material. The glass material is one or more compounds selected from Li2O, Li2S, Li2SO4, Li3PO4, B2O3, P2O5, P2O3, Al2O3, SiO2, CaO, MgO, BaO, TiO2, GeO2, SiS2, Sb2O3, SnS, TaS2, P2S5, B2S3, and a combination of two or more thereof. A lithium-ion conducting solid electrolyte composite is disclosed comprising a lithium-ion conductive substance of the general formula La2/3-xLi3xTiO3—Z wherein x ranges form about 0.04 to 0.17, and wherein “Z” is the glass material identified above. A battery is disclosed having at least one cathode and anode and an inorganic solid electrolyte glass phase composite as described above disposed on or between at least one of the cathode and the anode.
申请公布号 US8865354(B2) 申请公布日期 2014.10.21
申请号 US201113074335 申请日期 2011.03.29
申请人 West Virginia University 发明人 Zhang Hui;Jiang Yinglu;Liu Xingbo
分类号 H01M10/0562 主分类号 H01M10/0562
代理机构 Buchanan Ingersoll & Rooney PC 代理人 Buchanan Ingersoll & Rooney PC ;Cochenour Craig G.
主权项 1. An inorganic solid electrolyte composite comprising: La2/3-xLi3xTiO3 wherein x ranges from about 0.04 to about 0.17, and a glass material comprising B2O3 forming an inorganic solid electrolyte glass composite having a modified grain boundary of rounded non-cubic shaped grains and a grain boundary conductivity greater than about 9.03×10−6 S cm−1.
地址 Morgantown WV US