摘要 |
<p>Method of applying polymeric material on coated laminated composite plate involves applying layer (2) on composite sheet (1), applying silicon nitride layer (3) to layer (2), applying primer (4) on silicon nitride layer (3), and applying polymer to primer (4). The functional layer contains niobium, tantalum, molybdenum, zirconium, silver, gold, aluminum, nickel, chromium and/or copper. The dielectric layer contains silica, tin dioxide, bismuth oxide, zinc oxide, titanium dioxide, tantalum pentoxide, aluminum nitride and/or silicon nitride. Method of applying polymeric material on coated laminated composite plate involves applying layer containing functional layer (2a) and/or dielectric layer (2b), on a composite sheet, applying silicon nitride layer with thickness of 20-100 nm to the layer, applying primer on the silicon nitride layer, and applying polymer to the primer. The functional layer contains niobium, tantalum, molybdenum, zirconium, silver, gold, aluminum, nickel, chromium and/or copper. The dielectric layer contains silica, tin dioxide, bismuth oxide, zinc oxide, titanium dioxide, tantalum pentoxide, aluminum nitride and/or silicon nitride.</p> |