摘要 |
<p>A method of manufacturing a solar cell back side electrode comprising: (a) preparing a substrate comprising a semiconductor layer and a passivation layer formed on the back side of the semiconductor layer, wherein the passivation layer has one or more openings; (b) applying, onto the back side of the substrate, an aluminum paste comprising, (i) an aluminum powder, (ii) a glass frit comprising 30 to 70 cation mole percent of lead, 1 to 40 cation mole percent of silicon and 10 to 65 cation mole percent of boron, and 1 to 25 cation mole percent of aluminum, based on the total mole of cationic components in the glass frit, and (iii) an organic medium, wherein the aluminum paste covers the openings; and (c) firing the aluminum paste in a furnace, wherein the aluminum paste does not fire through the passivation layer during the firing.</p> |