<p>Polymer-modified polyol, for use as a starting material for polyurethane foam, is made by reacting an olamine, such as triethanolamine, with an isocyanate in the presence of a metal organic catalyst. The catalyst is a metal salt of an organic acid and the viscosity of the polymer-modified polyol is at least 2250 mPa·s. In one embodiment the catalyst is of the formulat M(O.CO.R.CH3)2 where M is a metal and R is a carbon chain of 6 to 20 carbons. A metal salt of a monohydroxy fatty acid, particularly ricinoleic acid may be used.</p> |
申请公布号 |
BRPI0809329(A2) |
申请公布日期 |
2014.09.09 |
申请号 |
BR2008PI09329 |
申请日期 |
2008.03.20 |
申请人 |
FRITZ NAUER AG |
发明人 |
HENRI MISPREUVE;REINOLD NAESCHER;KURT SCHOENENBERGER;JOHAN FREI;ERIK VOGEL;ZACHARIAS GROTE |
分类号 |
C08G18/12;C08G18/08;C08G18/16;C08G18/24;C08G18/32;C08G18/40;C08G18/48;C08G18/66 |
主分类号 |
C08G18/12 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|