摘要 |
<p>PROBLEM TO BE SOLVED: To provide a molding material capable of obtaining a molded product which is excellent in dispersibility of a carbon fiber to a polycarbonate resin when being molded, and can exhibit excellent fire retardancy and dynamic characteristics.SOLUTION: In a molding material containing a total 100 pts.wt. of the following components (A) to (D), the molding material is obtained by coating resin impregnated reinforcing fiber bundles (E) obtained by melting and impregnating the following component (B) into the following component (A), with the following component (C) and the following component (D). The components are (A) 5-35 pts.wt. of a carbon fiber to which a sizing agent containing an epoxy resin is attached in a range of 0.01-3.0 wt.%, (B) 1-15 pts.wt. of a phenolic resin, (C) 30-89 pts.wt. of a polycarbonate resin, and (D) 5-20 pts.wt. of a phosphorus flame-based retardant.</p> |