发明名称 FERRITE-AUSTENITE 2-PHASE STAINLESS STEEL PLATE HAVING LOW IN-PLANE ANISOTROPY AND METHOD FOR PRODUCING SAME
摘要 This ferrite austenite 2-phase stainless steel plate comprises, by mass%, C: 0.001-0.10%, Si: 0.01-1.0%, Mn: 2-10%, P <u><</u> 0.05%, Ni: 0.1-3.0%, Cr: 15.0-30.0%, and N: 0.05-0.30%, with the remainder being Fe and inevitable impurities. The austenite phase percentage is 40-90% by surface area percentage, the maximum strength of the crystal orientation of the ferrite phase is 10 or less, and the hardness ratio of the austenite phase to the ferrite phase is 1.1 or greater.
申请公布号 KR20140105849(A) 申请公布日期 2014.09.02
申请号 KR20147020498 申请日期 2013.03.05
申请人 NIPPON STEEL & SUMIKIN STAINLESS STEEL CORPORATION 发明人 HAMADA JUNICHI;ISHIMARU EIICHIRO
分类号 C22C38/58;C21D8/02;C22C38/50 主分类号 C22C38/58