发明名称 METHOD FOR SYNTHESIS OF BORON SUBOXIDE
摘要 Methods of preparing boron suboxide are provided herein. In some embodiments, a method for preparing boron suboxide may include loading elemental boron powder into a furnace; purging the furnace by flowing a first gas comprising one of nitrogen or an inert gas into the furnace; heating the boron powder in a reactive atmosphere comprising a mixture of argon and a non-reducing oxygen-containing gas to convert elemental boron powder into boron suboxide powder, wherein the amount of oxygen in the reactive atmosphere is no greater than about 1%.
申请公布号 US2014227158(A1) 申请公布日期 2014.08.14
申请号 US201313767358 申请日期 2013.02.14
申请人 U.S. ARMY RESEARCH LABORATORY ATTN: RDRL-LOC-I 发明人 Pavlacka Robert J.;Gilde Gary A.
分类号 C01B35/10 主分类号 C01B35/10
代理机构 代理人
主权项 1. A method of preparing a boron suboxide powder, comprising: loading elemental boron powder into a furnace; purging the furnace by flowing a gas selected from the group consisting of nitrogen or another inert gas and mixtures thereof into the furnace; heating the boron powder in a reactive atmosphere comprising a mixture of an inert gas and a non-reducing oxygen-containing gas to convert elemental boron powder into boron suboxide powder, wherein the amount of oxygen in the reactive atmosphere is no greater than about 1%; and removing the boron suboxide powder from the furnace.
地址 Adelphi MD US