发明名称 |
Low-charging fiber and method for producing the same |
摘要 |
An object to be achieved by the invention is to provide a biodegradable low-charging fiber. The prevent inventors have found that when a specific amount of a specific phospholipid that is not known to have antistatic properties is added to a biodegradable polymer, and the resulting mixture is formed into a fiber having a smooth surface, low-charging properties are developed. The invention has thus been accomplished. The invention is a fiber having an average surface porosity of less than 3% and made of a biodegradable polymer that contains a specific amount of a specific phospholipid. |
申请公布号 |
US8802756(B2) |
申请公布日期 |
2014.08.12 |
申请号 |
US201113816058 |
申请日期 |
2011.08.12 |
申请人 |
Teijin Limited |
发明人 |
Kageyama Yukako;Honda Susumu;Satake Makoto;Kaneko Hiroaki |
分类号 |
C08K5/52 |
主分类号 |
C08K5/52 |
代理机构 |
Sughrue Mion, PLLC |
代理人 |
Sughrue Mion, PLLC |
主权项 |
1. A fiber comprising a biodegradable polymer that contains a phospholipid and having an average surface porosity of less than 3%,
wherein the phospholipid is one of the following: dilauroylphosphatidylcholine in an amount of 0.2 wt % to 5 wt %; dimyristoylphosphatidylcholine in an amount of 0.4 wt % to 5 wt %; dipalmitoylphosphatidylcholine in an amount of 1 wt % to 5 wt %; dioleoylphosphatidylcholine in an amount of 1 wt % to 5 wt %; and dioleoylphosphatidylethanolamine in an amount of 1 wt % to 5 wt %; or is two or more of the phospholipids in a total amount of 5 wt % or less, and in a total amount of 1 wt % or more, or contains at least dilauroylphosphatidylcholine in an amount of 0.2 wt % or more, or contains at least dimyristoylphosphatidylcholine in an amount of 0.4 wt % or more. |