发明名称 Lithium-containing composite oxide and its production method
摘要 A lithium/nickel/cobalt/manganese-containing composite oxide powder represented by the formula LipNixCoyMnzMqO2-aFa (wherein M is at least one element selected from the group consisting of Al, Ge, Sn, alkaline earth metal elements and transition metal elements other than Co, Mn and Ni, 0.9≦p≦1.1, 0.2≦x≦0.5, 0.2≦y≦0.5, 0.1≦z≦0.4, 0≦q≦0.5, 1.9≦a≦2.1, p+x+y+z+q=2, and 0≦a≦0.02), characterized in that when the powder is classified into small particle size-classified particles with an average particle size 2 μm≦D50≦8 μm and large particle size-classified particles with an average particle size of 10 μm≦D50≦75 μm, the ratio of (% by weight of the small particle size-classified particles)/(% by weight of the large particle size-classified particles) is from 15/85 to 40/60.
申请公布号 US8795896(B2) 申请公布日期 2014.08.05
申请号 US200912486799 申请日期 2009.06.18
申请人 AGC Seimi Chemical Co., Ltd. 发明人 Kawasato Takeshi;Mihara Takuya;Ueda Koichiro;Wakasugi Yukimitsu;Honda Nozomi
分类号 H01M4/00;H01M4/36;H01M4/525;H01M4/131 主分类号 H01M4/00
代理机构 Oblon, Spivak, McClelland, Maier & Neustadt, L.L.P. 代理人 Oblon, Spivak, McClelland, Maier & Neustadt, L.L.P.
主权项 1. A lithium/nickel/cobalt/manganese-containing composite oxide powder represented by the formula LipNixCoyMnzMqO2-aFa wherein M is at least one element selected from the group consisting of A1, Ge, Sn, alkaline earth metal elements and transition metal elements other than Co, Mn and Ni, 0.9≦p≦1.1, 0.2≦x≦0.5, 0.2≦y≦0.5, 0.1≦z≦0.4, 0≦q≦0.5, 1.9≦a≦2.1, p+x+y+z+q=2, and 0≦a≦0.02, characterized in that when the powder is classified into small particle size-classified particles with an average particle size of 2 μm≦D50≦8 μm and large particle size-classified particles with an average particle size of 10 μm≦D50≦75 μm, a ratio of % by weight of the small particle size-classified particles compared to a % by weight of the large particle size-classified particles is from 15/85 to 40/60, a molar ratio ps of lithium to the total of nickel, cobalt, manganese and the M element contained in the small particle size-classified particles is smaller than a molar ratio pl of lithium to the total of nickel, cobalt, manganese and the M element contained in the large particle size-classified particles and wherein 0.95≦ps≦1.04, 1.03≦pl≦1.12, 0.85<ps/pl<1.
地址 Chigasaki JP