摘要 A method is employed for producing a positive electrode active material for a lithium secondary battery that comprises mixing lithium phosphate having a particle diameter D90 of 100 μm or less, an M element-containing compound having a particle diameter D90 of 100 μm or less (where, M is one type or two or more types of elements selected from the group consisting of Mg, Ca, Fe, Mn, Ni, Co, Zn, Ge, Cu, Cr, Ti, Sr, Ba, Sc, Y, Al, Ga, In, Si, B and rare earth elements) and water, adjusting the concentration of the M element with respect to water to 4 moles/L or more to obtain a raw material, and producing olivine-type LiMPO4 by carrying out hydrothermal synthesis using the raw material.
申请公布号 US2014203218(A1) 申请公布日期 2014.07.24
申请号 US201414223344 申请日期 2014.03.24
申请人 SHOWA DENKO K.K. 发明人 TONEGAWA Akihisa;SHIRAKAWA Akihiko;KABE Isao;ORIJI Gaku
分类号 C01B25/45;H01M4/1397;H01M4/04 主分类号 C01B25/45
代理机构 代理人
主权项 1. A method for producing a positive electrode active material for a lithium secondary battery, comprising: mixing lithium phosphate having a particle diameter D90 of 100 μm or less, an M element-containing compound having a particle diameter D90 of 100 μm or less (where, M is one type or two or more types of elements selected from the group consisting of Mg, Ca, Fe, Mn, Ni, Co, Zn, Ge, Cu, Cr, Ti, Sr, Ba, Sc, Y, Al, Ga, In, Si, B and rare earth elements) and water, adjusting the concentration of the M element with respect to water to 4 moles/L or more to obtain a raw material, and producing olivine-type LiMPO4 by carrying out hydrothermal synthesis using the raw material.
地址 Tokyo JP