发明名称 HEAT TREATMENT METHOD OF TURNOUT TRACK AND THE TURNOUT TRACK
摘要 The present invention provides a heat treatment method of turnout track comprising performing an accelerated cooling on the turnout track to be treated having a railhead tread with a temperature of 650-900° C. so as to obtain the turnout track with full pearlite metallographic structure, wherein the accelerated cooling velocity performed on the working side of railhead of the turnout track is higher than that performed on the non-working side of the railhead of the turnout track. The present invention provides a turnout track obtained with a heat treatment process as depicted therein. The turnout track in present invention has good straightness; both the hardness and tensile strength of the working side of railhead are higher than that of the non-working side of railhead.
申请公布号 US2014182751(A1) 申请公布日期 2014.07.03
申请号 US201314142268 申请日期 2013.12.27
申请人 Pangang Group Panzhihua Steel & Vanadium Co., Ltd. ;Pangang Group Panzhihua Iron & Steel Research Institute Co., Ltd. 发明人 Zou Ming;Han Zhenyu;Mei Dongsheng;Deng Yong;Guo Hua;Xu Quan;Wang Chunjian
分类号 C21D9/04;E01B7/00 主分类号 C21D9/04
代理机构 代理人
主权项 1. A heat treatment method of turnout track comprising performing an accelerated cooling on the turnout track to be treated having a railhead tread with a temperature of 650-900° C. so as to obtain the turnout track with full pearlite metallographic structure, wherein the accelerated cooling velocity performed on the working side of the railhead of the turnout track is higher than that performed on the non-working side of the railhead of the turnout track.
地址 Panzhihua CN