摘要 |
<p>Method for batch wise slaking of burnt lime in a slaker, in which a lime slurry is produced with a great degree of fineness and long sedimentation time, comprising the following steps: the regulation of the slaking temperature is carried out in either of two steps-at incoming water temperatures between 0-10° C. a predetermined amount of the finished slurry is emptied out-at incoming water temperatures between 10-20° C. a predetermined amount of flushing water or diluting water is added.</p> |