摘要 FIELD: metallurgy.SUBSTANCE: prior to inductive hard-facing of the charge, the part is subjected to preliminary hardening to the depth of 0.3-0.6 mm. Used charge consists of the mix of 20-30% of boron carbide and 70-80% of flux. Said mix in depth of 0.8-1.4 mm is applied on the part. Said charge is fused by high-frequency current and cured at, at least, 1240°C for 50-70 s.EFFECT: ruled out undesirable structures in the ply, hence, higher wear resistance.3 dwg, 1 ex
申请公布号 RU2520879(C1) 申请公布日期 2014.06.27
申请号 RU20120150001 申请日期 2012.11.22
申请人 FEDERAL'NOE GOSUDARSTVENNOE BJUDZHETNOE OBRAZOVATEL'NOE UCHREZHDENIE VYSSHEGO PROFESSIONAL'NOGO OBRAZOVANIJA "ALTAJSKIJ GOSUDARSTVENNYJ AGRARNYJ UNIVERSITET" (FGBOU VPO AGAU) 发明人 IVANAJSKIJ VIKTOR VASIL'EVICH;ISHKOV ALEKSEJ VLADIMIROVICH;KRIVOCHUROV NIKOLAJ TIKHONOVICH;SHANCHUROV SERGEJ MIKHAJLOVICH;SHAJKHUDINOV ALEKSANDR SERGEEVICH