发明名称 SOFT TISSUE HAVING REDUCED HYDROGEN BONDING
摘要 The present invention provides a modified cellulosic fiber having reduced hydrogen bonding capabilities. The modified fiber formed in accordance with the present invention may be useful in the production of tissue products having improved bulk and softness. More importantly, the modified fiber is adaptable to current tissue making processes and may be incorporated into a tissue product to improve bulk and softness without an unsatisfactory reduction in tensile.
申请公布号 US2014174686(A1) 申请公布日期 2014.06.26
申请号 US201213726938 申请日期 2012.12.26
申请人 KIMBERLY-CLARK WORLDWIDE, INC. 发明人 Yang SeungRim;Kim JeongKyung;Qin Jian
分类号 D21C1/04 主分类号 D21C1/04
代理机构 代理人
主权项 1. A method of increasing the bulk of a tissue web comprising the steps of reacting cellulosic fiber with a water soluble reagent selected from the group consisting of a cyanuric halide having the general Formula (I): where R1 equals F, Cl, Br, or I and R2 equals (CH2)n—OH (n=1-3), (CH2)n—COOH (n=1-3), C6H5—COOH, or HSO3X where X equals (CH2)n (n=1-3) or C6H4, and a vinyl sulfone having the general Formula (II): where R1 equals a hydrocarbon having from about 1 to about 5 carbon atoms and R2 equals CH3, HC═CH2, (CH2)n—CH3 (n=1-3), (CH2)n—COOH (n=1-3), C6H4—COOH, or C6H5; treating the cellulosic fiber with a caustic agent; washing the cellulosic fiber; and forming a tissue web from the cellulosic fiber, wherein the tissue web has a basis weight greater than about 10 grams per square meter (gsm) and a sheet bulk greater than about 5 cc/g.
地址 Neenah WI US