发明名称 Para-aromatic polyamide fiber and method for manufacturing the same
摘要 PURPOSE: A para-aromatic polyamide fiber and a manufacturing method thereof are provided to reduce crystallinity of a para-aromatic polyamide fiber and a crystal size to increase a moisture rate, thereby increasing a dyeing property. CONSTITUTION: Spinning dope is spun by a spinneret(10). The spun spinning dope is coagulated in a coagulation bath(20) through an air gap. A filament containing sulfuric acid is cleaned in the first water cleaning bath(30). The filament is cleaned in the second wafer cleaning bath(40). The first and second cleaning rollers(31,41) move the filament. A drying roller(51) eliminates moisture from the filament. A winder(60) ties the filament.
申请公布号 KR101410541(B1) 申请公布日期 2014.06.20
申请号 KR20090056873 申请日期 2009.06.25
申请人 发明人
分类号 D01F6/60;D04B1/14;D06P1/41;D06P3/24 主分类号 D01F6/60