发明名称 METHOD FOR PRODUCING PNEUMATIC TIRE, AND PNEUMATIC TIRE
摘要 <p>PROBLEM TO BE SOLVED: To provide a pneumatic tire in which fuel consumption performance and WET brake performance are made consistent by optimizing vulcanization temperature conditions, and a method for producing the same.SOLUTION: Provided is a method for producing a pneumatic tire including a vulcanization step where, provided that the temperature of the outer surface of a tread part in a vulcanization step is defined as To(°C) and the temperature of the outer surface of a side wall part is defined as So(°C), To/So=1.00 to 1.10 (1) is satisfied, and further, provided that the temperature of the inner surface of the tread part is defined as Ti(°C), To/Ti=0.70 to 0.90 (2) is satisfied.</p>
申请公布号 JP2014104649(A) 申请公布日期 2014.06.09
申请号 JP20120258853 申请日期 2012.11.27
申请人 TOYO TIRE & RUBBER CO LTD 发明人 NARITA HIROAKI
分类号 B29C33/02;B29C35/02;B29D30/06;B29L30/00 主分类号 B29C33/02
代理机构 代理人
主权项
地址
您可能感兴趣的专利